My Site
Skip to Content

New Superalloys Boost Direct Metal Laser Sintering

August 24, 2010

Leslie Gordon

Printer-friendly version
EOS GmbH – Electro Optical Systems, tinyurl.com/2cuwdcn

Often used in the additive building of prototypes, direct-metal laser sintering (DMLS) also works well in rapid manufacturing across a range of industries. This trend is supported by current advances in materials. For example, EOS GmbH – Electro Optical Systems, Munich, Germany, recently developed nickel superalloy EOS IN718 and aluminum alloy EOS AlSi10Mg. EOS IN718 is similar to Inconel 718, has excellent mechanical strength, and withstands high temperatures. The alloy provides good tensile, fatigue, creep, and rupture strength up to 1,292°F. Its excellent corrosion resistance makes the alloy suitable for parts ranging from fasteners and valves to aerospace gas turbines.

Inconel 718 has long been used for these kinds of components, but laser-sintered IN718 can provide a simpler solution because it eliminates machining. This is important because nickel alloys can be difficult to cut on a traditional machine tool.

IN718 can be heat treated following the same AMS 5662 and AMS 5664 standards that apply to Inconel alloys. Secondary operations that can be performed on DMLS parts include machining, spark-eroding, micro shot-peening, polishing, and coating.

Other nickel-based superalloys in the company’s pipeline for the future include EOS IN625, which is similar to Inconel 625.

EOS AlSi10Mg, on the other hand, contains aluminum, magnesium, and 9 to11% silicon to increase the material’s strength and hardness. It has properties similar to those of the traditional casting alloy. In both conventional and laser-sintered forms, the alloy retains aluminum’s light weight and high thermal conductivity. The additional elements give AlSi10Mg good casting properties, such as higher melt fluidity.

In its conventional form, AlSi10Mg often casts thin-walled, intricate parts. The laser-sintered form lets users build more-complex, lightweight parts with even thinner walls. Because DMLS rapidly solidifies parts, laser-sintered components have similar properties to conventional cast parts after T6 heat treatment. The laser-sintered parts can withstand secondary operations with EDM, welding, coating, polishing, wire eroding, and microblasting. Applications for the alloy include lightweight, load-bearing parts in motorsports, aerospace, and pneumatics.

© 2010 Penton Media, Inc.

Comments

Yes it is possible,

Yes it is possible, selective laser sintering machines a system with a system with a laser ray to mix selectively powdered matters, into a single firm object.

making parts

Dear Sir

Is it possible for your company to make my parts ?
If yes please inform me about the time and costs
for making some parts with inchonel718 with these Dimensions :153mm*153mm*120mm.
If needed we can send you indeed informations ;like technical
requiremaemts of our parts.

Sincerely Yours
Majid

Hi Majid, I can get you

Hi Majid,
I can get you machined on inconel 718 in Canada. Please get me more info to joshuakuriakose@gmail.com

Buildind a part from incl 718

Dear Sir

We want to buy a DMLS machine for making some parts from inchonel 718 .
PLease inform me how can I buy one .
The bigest dimensions of my parts is 20*20*20 cm .

Best Regards
Majid

Leave a comment

The content of this field is kept private and will not be shown publicly.

Acceptable Use Policy