Flexible, High Thermal Conductivity Epoxy
EP21TDC-2LO has a thermal conductivity of 9 Btu/in./ft2/hr/°F and a volume resistivity of over 1012 Ω-cm.
EP21TDC-2LO has a thermal
conductivity of 9 Btu/in./ft2/hr/°F and a
volume resistivity
of over 1012 Ω-cm. It has a 1:3 mix
ratio by weight or
volume, over
90 min of work life
(for a 100-gm
mass), and cures at
room temperatures or more rapidly
with heat to 36 Shore D hardness. It
withstands temperatures from –453 to
250°F, has an elongation of >50%, and
tensile and T-peel strengths of 1.07
kpsi and >15 pli, respectively.
Master Bond Inc.,
154 Hobart St.,
Hackensack, NJ 07601,
(201) 343-8983,
masterbond.com